Mathew, M D
(Elsevier, 2014)
P92 steel was normalized at 1353 K for 30 minutes followed by air cooling and subsequently tempered at 1013, 1033 and 1053 K for 60 minutes each followed by air cooling. The effect of tempering temperatures on the tensile ...